Name both surfaces at the interface
Before wrapping, label the two faces on the sample and identify which face points toward the pallet. Then record the two faces meeting at an overlap or tail. When neighboring loads touch, the exposed face of each load forms a separate pairing.
Agree with the supplier how its roll labels define the cling side. A report that names only a cling value leaves the surface pairing unresolved.
Read the scope of the peel test
ASTM D5458 covers peel cling between layers of stretch wrap film. Ask the lab for the method edition, contact surfaces, specimen preparation and the reported stretch condition. Keep force or force-per-width units exactly as the report defines them.
Ask the lab to apply the full method and document any departure. When the sheet contains more than one condition, compare results from matching conditions and retain the rest for context.
Record the state of the film in use
- Film ID and lot, time in storage and wrapping area temperature.
- Film stretch, overlap and tail placement, including the actual faces in contact.
- Any dust, moisture or other visible contamination, and the delay between wrapping and inspection.
Example: If a fresh sample holds securely in the trial area but the tail lifts after storage, repeat with the recorded storage and closing conditions and examine the tail interface before changing grades.
Set an observation for each contact
| Use case | Acceptance evidence to agree |
|---|---|
| Tail retention | Tail position and acceptable lift at defined handling checkpoints, with the same closing procedure across samples. |
| Adjacent loads | A documented contact arrangement or emulation followed by separation. Record any snagging, cover damage or transfer marks. |
A cling change that helps the tail can alter how adjoining loads separate. Review both observations when the expected storage arrangement includes load-to-load contact.