Keep the point where it started
Photograph the break before discarding the film. Capture a wider view showing the load face and a close-up around the earliest known damage. Save a strip that includes the suspected origin, and mark travel direction, inside and outside, roll ID and time.
If the origin is uncertain, mark it as suspected and record what the operator saw first. Keep an intact sample from the same roll to compare edges and surfaces.
Inspect the roll and web path
- Check both roll edges for crushed spots, notches or layers displaced during handling.
- Record where the web passes guides, and whether the tear aligns with a point on the path or the load.
- Have qualified staff inspect machine contact points with equipment secured according to the manufacturer’s procedure. Capture the corresponding position on the film.
Distinguish initiation from propagation
| Question | Useful evidence |
|---|---|
| Where did the tear begin? | A notch, initial hole or contact mark, location and when it first appeared. |
| How did it spread? | Direction relative to MD and TD, tear length and whether the spread occurred during wrapping or handling. |
| Which lab check fits? | A puncture check can help compare resistance to a probe. An agreed tear-propagation method such as ASTM D1922 measures propagation behavior in its specified setup. |
The two observations help narrow what to change. A long tear can grow from a small pre-existing defect.
Retest one correction at a time
Example: If the break repeatedly starts from a nick near one roll edge, repeat the same program with an undamaged reference roll and separately review roll transport and handling. If the break follows a load corner across both rolls, run a separate trial with a protected corner.
Record whether the origin recurs, which opportunities there were for a repeat and whether the rest of the wrap remained acceptable. A result tied to the same program and load is easier to interpret.